Considerations for the weldability of types 304L and 316L stainless steel PS Korinko, SH Malene Practical failure analysis 1, 61-68, 2001 | 108 | 2001 |
Evaluation of oxidation and hydrogen permeation in Al-containing stainless steel alloys TM Adams, P Korinko, A Duncan Materials Science and Engineering: A 424 (1-2), 33-39, 2006 | 44 | 2006 |
Method for electrophoretic deposition of brazing material PS Korinko, ML Hunt US Patent 5,976,337, 1999 | 35 | 1999 |
Laser engineered net shaping® for repair and hydrogen compatibility P Korinko, T Adams, S Malene, D Gill, J Smugeresky Weld. J 90 (9), 171s-181s, 2011 | 27 | 2011 |
Improved performance rhenium containing single crystal alloy turbine blades utilizing PPM levels of the highly reactive elements lanthanum and yttrium DA Ford, KPL Fullagar, HK Bhangu, MC Thomas, PS Burkholder, ... | 23 | 1999 |
Simulations of fracture tests of uncharged and hydrogen-charged additively manufactured 304 stainless steel specimens using cohesive zone modeling SJ Sung, J Pan, PS Korinko, M Morgan, A McWillliams Engineering Fracture Mechanics 209, 125-146, 2019 | 18 | 2019 |
Enhancement of coating uniformity by alumina doping GE Creech, PS Korinko, MJ Barber, SK Naik US Patent 5,958,204, 1999 | 17 | 1999 |
Nanoparticle treated stainless steel filters for metal vapor sequestration SEH Murph, GK Larsen, P Korinko, KJ Coopersmith, AJ Summer, R Lewis JOM 69, 162-172, 2017 | 16 | 2017 |
One-step noble metal-aluminide coatings GE Creech, SK Naik, PS Korinko US Patent 6,406,561, 2002 | 16 | 2002 |
Hydrogen permeation resistant coatings P Korinko, T Adams, G Creech Savannah River Site (SRS), Aiken, SC, 2005 | 12 | 2005 |
Analysis of zinc 65 contamination after vacuum thermal process PS Korinko, MH Tosten Journal of failure analysis and prevention 13, 389-395, 2013 | 11 | 2013 |
The role of partial crystallinity on hydrogen permeation in Fe–Ni–B–Mo based metallic glass membranes K Brinkman, E Fox, P Korinko, D Missimer, T Adams, D Su Journal of membrane science 378 (1-2), 301-307, 2011 | 10 | 2011 |
Coating Characterization and Evaluation of Directionally Solidified CM 186 LC® and Single Crystal CMSX-4® PS Korinko, MJ Barber, M Thomas Turbo Expo: Power for Land, Sea, and Air 78767, V005T12A005, 1996 | 10 | 1996 |
Modeling of crack extensions in arc-shaped specimens of hydrogen-charged austenitic stainless steels using cohesive zone model S Wu, SJ Sung, J Pan, PS Lam, MJ Morgan, PS Korinko Pressure Vessels and Piping Conference 51678, V06AT06A020, 2018 | 9 | 2018 |
Characterization of additive manufacturing for process tubing PS Korinko, JT Bobbitt, MJ Morgan, M Reigel, FA List, SS Babu JOM 71, 1095-1104, 2019 | 8 | 2019 |
Proton conducting ceramics in membrane separations KS Brinkman, PS Korinko, EB Fox, F Chen US Patent 9,005,486, 2015 | 7 | 2015 |
Methods of preventing the spread of zinc contamination during vacuum processing PS Korinko, AJ Duncan, KJ Stoner Journal of Failure Analysis and Prevention 14, 113-121, 2014 | 7 | 2014 |
Reactive Gas Recycle for Used Nuclear Fuel J Gray, P Korinko, B Garcia-Diaz, A Visser, T Adams FCRD Annual Report, FCRD-SEPA-2010-000177, 2010 | 7 | 2010 |
Comparison of ring compression testing to three point bend testing for unirradiated ZIRLO cladding PS Korinko, RL Sindelar, RL Kesterson Pressure Vessels and Piping Conference 57021, V007T07A055, 2015 | 6 | 2015 |